Polymer Property : Moisture Vapor Transmission = 6.00 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 6.00 cc-mm/m²-24hr-atm
15.2 cc-mil/100 in²-24hr-atm
F 372 Test conducted at 38°C (100°F) and 100% relative humidity.
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..