Polymer Property : Specific Heat Capacity = 0.490 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-105C PET Bottle Grade
A co-polymer used for soft drinks and other applications.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-109JS PET Sheet Grade
Used mainly for 5 to 20 liter mineral water containers
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-113C PET Sheet Grade
Used mainly for box strapping.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET D-101-SH Monofilament Resin
Used in the paper industry as paper pulp nets.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET F096H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET F096HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET F097H Film Grade Resin
Used mainly as PET films/ sheets, known as Superbright
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET F097HA Film Grade Resin
Used mainly as PET films/ sheets, known as bright with anti-blocking agent.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET FR-101-H Monofilament Resin
Used as textile grade flame retardant for furniture, car and plane upholstery.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy  (discontinued **)
Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-07C PET Bottle Grade
A co-polymer used mostly for containers.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-101C PET Sheet Grade
A sheet grade polymer used in thick films.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B101H Monofilament Resin
Generally used in monofilament v-belts, zips and other technical applications.
Specific Heat Capacity 2.05 J/g-°C

@Temperature 280 °C
0.490 BTU/lb-°F

@Temperature 536 °F
Pearl Engineering PEPLPET B-103C PET Bottle Grade
A co-polymer used for mineral water bottles
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Cadence™ GS1 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Cadence™ GS2 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Cadence™ GS3 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Cadence™ GS4 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Drystar 0601 Copolyester, Injection Molded
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 240 °C
0.490 BTU/lb-°F

@Temperature 464 °F
DSC
Eastman Eastar MN004 Copolyester
Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl..
Specific Heat Capacity 2.05 J/g-°C

@Temperature 250 °C
0.490 BTU/lb-°F

@Temperature 482 °F
DSC
Eastman Eastman 1223 Copolyester
Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card..