Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
|
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |