Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 1.90 GPa | 276 ksi | ASTM D882 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |