Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ 5209 FPL 20 Natural Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ MD 4245-59770 Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPH-20C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.693 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AT-10CF/000 Acetal (POM) Copolymer Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.17 mm |
0.693 ft-lb/in @Thickness 0.125 in |
|
Nilit Polynil® N66-P50N Lubed Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -40.0 °C |
0.693 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Izod Impact, Notched | 0.370 - 2.03 J/cm | 0.693 - 3.80 ft-lb/in | Average value: 0.913 J/cm Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -40.0 °C |
0.693 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
BASF Capron® 8224 HSL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene Clarified, e-beam and Gamma radiation sterilizable and Autoclavable. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - Lab ware, Pipette tips.In.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL003 Acetal Copolymer LNP LUBRICOMP* KL003 is a compound based on Acetal Copolymer resin containing 15% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 (Asia Pacific) LNP* Lubricomp* RP003 is a compound based on Nylon 66 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815 PBT 15% GR PBT+ PET, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS (Asia Pacific) LNP* Thermocomp* CF008 is a compound based on Polystyrene resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific) LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP (Asia Pacific) LNP* THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006SXP PA 66 LNP* THERMOCOMP* RZ006SXP is a compound based on Nylon 66 resin containing 30% Milled Glass. Added feature of this material is: Heat Stabilized. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WF006SXC PBT LNP* Thermocomp* WF006SXC is a compound based on PBT containing Glass FIber. Characteristic of this grade is: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 815 PBT (Asia Pacific) 15% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature 23.0 °C |
0.693 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly (Asia Pacific) LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WH0245A PBT (Asia Pacific) LNP THERMOCOMP* WH0245A is a compound based on Polybutylene Terephalate resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -30.0 °C |
0.693 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Izod Impact, Notched | 0.370 J/cm @Temperature -30.0 °C |
0.693 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520.. |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
Total PPC M6823MZ Metallocene Isostatic Propylene Polymer TOTAL Petrochemicals Polypropylene M6823MZ is an isostatic form of copolymer polypropylene made via TOTAL Petrochemicals proprietary metallocene catalyst technology.Clarity. M6823MZ incorporates th.. |
|||
Izod Impact, Notched | 0.370 J/cm @Thickness 3.17 mm |
0.693 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPH-CC40 Natural Homopolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Izod Impact, Notched | 0.370 J/cm | 0.693 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 626 Nylon 6/6, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |