Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.97 J/g-°C @Temperature 37.8 °C |
0.470 BTU/lb-°F @Temperature 100 °F |
|
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
|
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.470 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Cadence™ GS1 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.470 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Cadence™ GS2 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.470 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Cadence™ GS3 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.470 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Cadence™ GS4 Copolyester for film calendering Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 200 °C |
0.471 BTU/lb-°F @Temperature 392 °F |
DSC |
Eastman Eastman 1223 Copolyester Applications:Blown filmCredit cardsDebit cardsDeodorant packagingElectronic packagingFabricated boxesFlexible packagingFood packagingFurniture/Furniture trimGaming cardsGift cardsIdentification card.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 37.8 °C |
0.470 BTU/lb-°F @Temperature 100 °F |
|
Duratherm 600 Paraffinic Heat Transfer Fluid Duratherm 600 - thermal fluid rated to 600°F it contains the industries most aggressive blend of additives for long, trouble free operation in a variety of applications. Specifically engineered to .. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 37.8 °C |
0.470 BTU/lb-°F @Temperature 100 °F |
|
Duratherm G Polyalkylenev Glycol Heat Transfer Fluid Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improv.. |
|||
Specific Heat Capacity | 1.97 J/g-°C @Temperature 204 °C |
0.472 BTU/lb-°F @Temperature 400 °F |
|
Duratherm S Silicone Heat Transfer Fluid Duratherm S - a silicone based heat transfer fluid that is ideally suited for high oxidation or completely exposed systems up to 650°F. Duratherm S is virtually impervious to oxidation and offers s.. |