Aremco AREMCOLOX™ 502-1100 (Full-Fired) Dense Alumino-Silicate |
Aluminum Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1100 (Unfired) Machinable Alumino-Silicate |
Aluminum Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina |
Aluminum Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1400 (Full-Fired) Dense Alumina |
Aluminum Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1600 (99%) Machinable Boron Nitride 99% |
Nitride |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1900-MTTZ Dense MgO Partially Stabilized Zirconium Oxide |
Zirconium Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide |
Zirconium Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1900-ZTA Dense Zirconia-Toughened Aluminum Oxide |
Aluminum Oxide |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-400 Machinable Glass Ceramic |
Machinable Ceramic |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic |
Machinable Ceramic |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide |
Machinable Ceramic |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-800 Macor Glass Ceramic
(Unverified Data**) |
Machinable Ceramic |
|
Aremco Aremco-Seal™ 613 High Temperature Glass Coating |
Ceramic/Metallic Coating |
Aremco-Seal™
|
Aremco Aremco-Seal™ 613 High Temperature Specialty Coatings Glass |
Glass |
Aremco-Seal™
|
Aremco Aremco-Seal™ 617 High Temperature Glass Coating |
Ceramic/Metallic Coating |
Aremco-Seal™
|
Aremco Ceramabind™ 542 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 642 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 642-A High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 643-2 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 644-A High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 644-S High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 830 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 875 High Temperature Inorganic Binder |
Potting/Casting Ceramic |
Ceramabind™
|
Aremco Ceramabind™ 880 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled |
Zirconium Oxide |
Ceramabond™
|
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled |
Magnesium Oxide |
Ceramabond™
|
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled |
Silicon Oxide |
Ceramabond™
|
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled |
Silicon Oxide |
Ceramabond™
|
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled |
Zirconium Oxide |
Ceramabond™
|
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled |
Zirconium Oxide |
Ceramabond™
|
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled |
Zirconium Oxide |
Ceramabond™
|
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 575-N High Temperature Potting & Casting Material Alumina |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 646-N High Temperature Potting & Casting Material Zirconia |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 673 Castable Ceramic |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 673-N High Temperature Potting & Casting Material Silicon Carbide |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacast™ 675-N High Temperature Potting & Casting Material Aluminum Nitride |
Nitride |
Ceramacast™
|
Aremco Ceramacast™ 895 High Temperature Potting & Casting Material Alumina |
Aluminum Oxide |
Ceramacast™
|
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate |
Zirconium Oxide |
Ceramacast™
|
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP3015-GR High Temperature Protective Coating Inorganic, Mixed Oxides Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP3015-WH High Temperature Protective Coating Inorganic, Mixed Oxides Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP5000 High Temperature Protective Coating Inorganic, Zinc Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Glass-Coat™ GC4000 High Temperature Specialty Coatings Glass |
Glass |
Glass-Coat™
|
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled |
Boride |
Graphi-Coat™
|
Aremco HiE-Coat™ 840-C High Emissivity Coating, Inorganic-Ceramic Filled |
Ceramic/Metallic Coating |
HiE-Coat™
|
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled |
Ceramic/Metallic Coating |
HiE-Coat™
|
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled |
Ceramic/Metallic Coating |
HiE-Coat™
|
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled |
Ceramic/Metallic Coating |
HiE-Coat™
|
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating |
Ceramic |
HiE-Coat™
|
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating |
Aluminum Oxide |
Pyro-Paint™
|
Aremco Pyro-Paint™ 634-AS High Temperature Refractory Coating |
Aluminum Oxide |
Pyro-Paint™
|
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating |
Nitride |
Pyro-Paint™
|
Aremco Pyro-Paint™ 634-SIC High Temperature Refractory Coating |
Carbide |
Pyro-Paint™
|
Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95% |
Zirconium Oxide |
Pyro-Paint™
|
Aremco Pyro-Putty™ 1500 High Temperature Ceramic-Metallic Putty, Ceramic Filled |
High Temp Ceramic Resin |
Pyro-Putty™
|
Aremco Pyro-Putty™ 2400 High Temperature Ceramic-Metallic Putty, Stainless Filled |
High Temp Ceramic Resin |
Pyro-Putty™
|
Aremco Pyro-Putty™ 653 High Temperature Ceramic-Metallic Putty, Stainless Filled |
High Temp Ceramic Resin |
Pyro-Putty™
|
Aremco Quartz-Coat™ 845 High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Quartz-Coat™
|
Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94% |
Nitride |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride |
Nitride |
AREMCOLOX™
|
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC |
Machinable Ceramic |
AREMCOLOX™
|
Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass |
Glass |
Aremco-Seal™
|
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder |
Ceramic |
Ceramabind™
|
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled |
Aluminum Oxide |
Ceramabond™
|
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled |
Nitride |
Ceramabond™
|
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled |
Carbide |
Ceramabond™
|
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound |
Potting/Casting Ceramic |
Ceramacast™
|
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica |
Potting/Casting Ceramic |
Ceramacoat™
|
Aremco Ceramacoat™ 845-BLK High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-GLT High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-GRY High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-SIL High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Ceramacoat™ 845-WHT High Temperature Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Ceramacoat™
|
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Cerama-Dip™
|
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Cerama-Dip™
|
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating |
Ceramic/Metallic Coating |
Cerama-Dip™
|
Aremco Corr-Paint™ CP2000 High Temperature Protective Coating Urethane, Carbon Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP2010 High Temperature Protective Coating Urethane, Aluminum Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled |
Ceramic/Metallic Coating |
Corr-Paint™
|
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass |
Glass |
Glass-Coat™
|
Aremco Pyro-Paint™ 634-AL High Temperature Refractory Coating |
Aluminum Oxide |
Pyro-Paint™
|