Material Notes:
Good thermal and dielectric properties and can be fired to increase temperature resistance and mechanical strength. Easily machined to close tolerances. Plates, rods and bars available to 12".
Physical Properties Metric English Comments
Specific Gravity 2.40 g/cc
2.40 g/cc
Porosity 2.6 %
2.6 %
Mechanical Properties Metric English Comments
Hardness, Mohs 1.0 - 2.0
1.0 - 2.0
Flexural Strength 31.0 MPa
4500 psi
Compressive Strength 82.7 MPa
12000 psi
Thermal Properties Metric English Comments
CTE, linear 4.50 µm/m-°C

@Temperature 20.0 °C
2.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 1.59 W/m-K
11.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 538 °C
1000 °F
Electrical Properties Metric English Comments
Dielectric Constant 5.8

@Frequency 1e+6 Hz
5.8

@Frequency 1e+6 Hz
Dielectric Strength 3.15 kV/mm
80.0 kV/in
Dissipation Factor 0.060

@Frequency 1e+6 Hz
0.060

@Frequency 1e+6 Hz