Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Aremco
Trade Name Ceramabond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and do not outgas after curing. They are also environmentally safe, non-flammable materials which contain no volatile organic compounds.General Features: High Adhesive Strength Bonding: Ceramic to Ceramic, Ceramic to Metal, Metal to Metal Principal Use: Textiles, Threadlocking
Physical Properties Metric English Comments
Density 1.80 - 1.95 g/cc
0.0650 - 0.0704 lb/in³
Volatile Organic Compounds (VOC) Content 0.000 g/l
0.000 g/l
Viscosity 2500 - 5000 cP
2500 - 5000 cP
Mechanical Properties Metric English Comments
Impact Test 81.3 J
60.0 ft-lb
Torque Strength; curing at 1000°F
Thermal Properties Metric English Comments
CTE, linear 7.74 µm/m-°C
4.30 µin/in-°F
Maximum Service Temperature, Air 1650 °C
3000 °F
Electrical Properties Metric English Comments
Dielectric Strength 5.59 kV/mm
142 kV/in
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
preceeded by 1-4 hour air set
Shelf Life 6.00 Month

@Temperature 4.44 - 32.2 °C
6.00 Month

@Temperature 40.0 - 90.0 °F
Descriptive Properties Value Comments
Acid Resistance Good
after curing at 700°F for 2 hours
Alkali Resistance Good
after curing at 700°F for 2 hours
Color White
Moisture Resistance Excellent
after curing at 700°F for 2 hours
Solvent Water
Thinner 670-T