Material Notes:
A colloidal silica aqueous solution which produces high adhesive strength. Ideal for blending with all types of granular and fibrous ceramics. Excellent resistance to temperature, moisture and mechanical shock.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
Solids Content 40 %
40 %
by weight
pH 9.0
9.0
Viscosity 35 cP
35 cP
Storage Temperature 7.22 - 35.0 °C
45.0 - 95.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1760 °C
3200 °F
Processing Properties Metric English Comments
Shelf Life 6.00 Month
6.00 Month