Material Notes:
High Temperature, water-dispersible silicone resin for producing corrosion and moisture resistant coatings and sealing porous ceramics. Cures at 450 °F in one hour.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Solids Content 50 %
50 %
by weight
pH 6.5
6.5
Viscosity 480 cP
480 cP
Storage Temperature 7.22 - 35.0 °C
45.0 - 95.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 649 °C
1200 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 232 °C
1.00 hour

@Temperature 450 °F
Shelf Life 6.00 Month
6.00 Month