Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94%

Category Ceramic , Machinable Ceramic , Nitride
Manufacturer Aremco
Trade Name AREMCOLOX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco AREMCOLOX™ 502-1600 (94%) Machinable Boron Nitride 94%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hot-pressed 94% boron nitride. High thermal conductivity. Easily machined. Non-reactive in molten salts, aluminum and other metals. Plates from 1/4" to 1" thick; rods from 1/4" to 3" diameter; bars from 1/4" x 1/4" to 2"x 2".
Physical Properties Metric English Comments
Specific Gravity 1.90 g/cc
1.90 g/cc
Porosity 11 %
11 %
Mechanical Properties Metric English Comments
Flexural Strength 51.7 MPa
7500 psi
Compressive Strength 68.9 MPa
10000 psi
Thermal Properties Metric English Comments
CTE, linear 3.96 µm/m-°C

@Temperature 20.0 °C
2.20 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 55.00 W/m-K
381.7 BTU-in/hr-ft²-°F
Maximum Service Temperature, Inert 1150 °C
2100 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.1

@Frequency 1e+6 Hz
4.1

@Frequency 1e+6 Hz
Dielectric Strength 52.8 kV/mm
1340 kV/in
Dissipation Factor <= 0.00020

@Frequency 1e+6 Hz
<= 0.00020

@Frequency 1e+6 Hz
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved