Material Notes:
Glass-enamel, gloss-black coating for stainless steel to 1000°F (538°C)
Physical Properties Metric English Comments
Specific Gravity 1.65 g/cc
1.65 g/cc
Solids Content 37.8 %
37.8 %
by volume
62.2 %
62.2 %
by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Viscosity 200 - 400 cP
200 - 400 cP
Thickness 25.4 microns
1.00 mil
Dry Film
67.1 microns
2.64 mil
Wet Film
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 538 °C
1000 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 1.77 kV/mm
45.0 kV/in
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 30.0 min
0.500 hour
Air Set prior to curing
10.0 min

@Temperature 200 °C
0.167 hour

@Temperature 392 °F
20 min at 1000°F, 3 min at 1300°F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Black
Theoretical Dry Film Coverage, ft2/gal 607
at 1 mil
Thinner Butyl Cellosolve/Water