Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica

Category Ceramic , Oxide , Silicon Oxide , Potting/Casting Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Aremco
Trade Name Ceramacoat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C)
Physical Properties Metric English Comments
Density 1.98 g/cc
0.0715 lb/in³
Solids Content 55.0 %
55.0 %
Volume
75.9 %
75.9 %
Weight
Volatiles 0.000 %
0.000 %
Viscosity 60000 - 80000 cP
60000 - 80000 cP
Thickness 25.4 microns
1.00 mil
Dry Film
46.2 microns
1.82 mil
Wet Film
Storage Temperature 55.0 - 85.0 °C
131 - 185 °F
Thermal Properties Metric English Comments
CTE, linear 9.90 µm/m-°C

@Temperature 20.0 °C
5.50 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 1320 °C
2400 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 6.30 kV/mm
160 kV/in
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Dry Time 2 - 4 hour
2 - 4 hour
Air dry
Cure Time 1440 min

@Temperature 23.0 °C
24.0 hour

@Temperature 73.4 °F
12000 min

@Time 7200 - 14400 sec
200 hour

@Time 2.00 - 4.00 hour
1st cure
21000 min

@Time 3600 - 7200 sec
350 hour

@Time 1.00 - 2.00 hour
2nd cure
30000 min

@Time 3600 sec
500 hour

@Time 1.00 hour
3rd cure
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Off-White
attacked by HF
Theoreticaly Dry Film Coverage 21.6 m2/liter
Thinner 521-N-T