Category Ceramic , Nitride , Potting/Casting Ceramic
Manufacturer Aremco
Trade Name Ceramacast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine grain aluminum nitride castable with high thermal conductivity
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Porosity <= 3.0 %
<= 3.0 %
Viscosity 12000 cP
12000 cP
Thickness 12.7 microns
0.500 mil
0
Mechanical Properties Metric English Comments
Compressive Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
CTE, linear 5.22 µm/m-°C

@Temperature 20.0 °C
2.90 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 1200 °C
2200 °F
Shrinkage <= 0.300 %

@Temperature 538 °C
<= 0.300 %

@Temperature 1000 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Strength 11.8 kV/mm
300 kV/in
Processing Properties Metric English Comments
Dry Time >= 8 hour
>= 8 hour
Air dry
Cure Time 300 - 420 min
5.00 - 7.00 hour
2-4 hrs at 200°F; 3 hrs at 250°F
Pot Life 60 - 120 min
60 - 120 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Acid Resistance Good
attacked by HF
Alkali Resistance Good