Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Ceramabind™ 542 High Temperature Inorganic Binder

Category Ceramic
Manufacturer Aremco
Trade Name Ceramabind™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramabind™ 542 High Temperature Inorganic Binder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Single part, low viscosity, water-dispersed, aluminum phosphate solution for penetrating ultra fine thermal spray applications to 3000°F (1650°C).
Physical Properties Metric English Comments
Specific Gravity 1.47 g/cc
1.47 g/cc
Solids Content 22.0 %
22.0 %
by volume
41.0 %
41.0 %
by weight
Volatile Organic Compounds (VOC) Content 0.000 g/l
0.000 g/l
pH 2.50
2.50
Viscosity 35.0 - 45.0 cP
35.0 - 45.0 cP
Thickness 25.4 microns
1.00 mil
dry film
115 microns
4.54 mil
wet film
Storage Temperature 55.0 - 85.0 °C
131 - 185 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 1650 °C
3000 °F
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Cure Time 60.0 - 120 min
1.00 - 2.00 hour
Air Set prior to curin
60.0 min

@Temperature 93.3 °C
1.00 hour

@Temperature 200 °F
500°F at 1 hr, 700°F at 1 hr
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Clear
Theoretical Dry Film Coverage, ft2/gal 353
at 1 mil
Thinner Water
Users viewing this material also viewed the following: