Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride

Category Ceramic , Machinable Ceramic , Nitride
Manufacturer Aremco
Trade Name AREMCOLOX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hot-pressed boron nitride – aluminum nitride composite that demonstrates high thermal conductivity, dielectric strength, and abrasion resistance. Readily machined and available in rods from 1/4” to 1” diameter x 12” long and plates from 1/4” to 1” thick by 5” x 5”.
Physical Properties Metric English Comments
Specific Gravity 2.43 g/cc
2.43 g/cc
Porosity 9.0 %
9.0 %
Mechanical Properties Metric English Comments
Flexural Strength 125 MPa
18200 psi
Thermal Properties Metric English Comments
CTE, linear 5.58 µm/m-°C
3.10 µin/in-°F
Thermal Conductivity 40.0 W/m-K
278 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 649 °C
1200 °F
Maximum Service Temperature, Inert 1200 °C
2200 °F
Electrical Properties Metric English Comments
Dielectric Constant 6.4

@Frequency 1.00e+6 Hz
6.4

@Frequency 1.00e+6 Hz
Dielectric Strength 42.9 kV/mm
1090 kV/in