Material Notes:
Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devices as well as high temperature fixtures, molds and tooling.
Physical Properties Metric English Comments
Bulk Density 1.73 g/cc
0.0625 lb/in³
Powder
Porosity <= 2.0 %
<= 2.0 %
pH 2.0 - 3.0
2.0 - 3.0
Viscosity 9000 cP
9000 cP
Mixed. Powder:liquid ratio is 100: 12-14
Mechanical Properties Metric English Comments
Compressive Strength 70.3 MPa
10200 psi
Thermal Properties Metric English Comments
CTE, linear 7.38 µm/m-°C

@Temperature 20.0 °C
4.10 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage <= 0.300 %

@Temperature 538 °C
<= 0.300 %

@Temperature 1000 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 5.91 kV/mm
150 kV/in
Processing Properties Metric English Comments
Dry Time >= 8 hour
>= 8 hour
Air dry
Cure Time 300 - 420 min
5.00 - 7.00 hour
2-4 hrs at 200°F; 3 hrs at 250°F
Pot Life 60 - 120 min
60 - 120 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Acid Resistance Good
attacked by HF
Alkali Resistance Good
Color White
Moisture Resistance Good