Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled

Category Ceramic , Oxide , Silicon Oxide
Manufacturer Aremco
Trade Name Ceramabond™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and do not outgas after curing. They are also environmentally safe, non-flammable materials which contain no volatile organic compounds.General Features: Low CTE, Good Strength Bonding: Ceramic to Ceramic, Quartz Principal Use: Tubes, Vessels, Sensors
Physical Properties Metric English Comments
Density 1.80 - 1.90 g/cc
0.0650 - 0.0686 lb/in³
Volatile Organic Compounds (VOC) Content 0.000 g/l
0.000 g/l
Viscosity 40000 - 60000 cP
40000 - 60000 cP
Mechanical Properties Metric English Comments
Impact Test 104 J
77.0 ft-lb
Torque Strength; curing at 1000°F
Thermal Properties Metric English Comments
CTE, linear 0.594 µm/m-°C
0.330 µin/in-°F
Maximum Service Temperature, Air 1650 °C
3000 °F
Electrical Properties Metric English Comments
Dielectric Strength 6.14 kV/mm
156 kV/in
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
Step 1, preceeded by 1-4 hour air set
120 min

@Temperature 260 °C
2.00 hour

@Temperature 500 °F
Step 2
120 min

@Temperature 371 °C
2.00 hour

@Temperature 700 °F
Step 3
Shelf Life 6.00 Month

@Temperature 4.44 - 32.2 °C
6.00 Month

@Temperature 40.0 - 90.0 °F
Descriptive Properties Value Comments
Acid Resistance Good
Alkali Resistance Good
Color Off-White
Moisture Resistance Excellent
Solvent Water
Thinner 618-N-T