Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina

Category Ceramic , Machinable Ceramic , Oxide , Aluminum Oxide
Manufacturer Aremco
Trade Name AREMCOLOX™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco AREMCOLOX™ 502-1400 (Bisque-fired) Machinable Alumina.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good corrosion electrical and thermal shock resistance. Plates from 1/4" to 3/4" thick; rods from 1/4" to 3" diameter. Easily machined using conventional tools, no firing required.
Physical Properties Metric English Comments
Specific Gravity 3.00 g/cc
3.00 g/cc
Porosity 25 %
25 %
Mechanical Properties Metric English Comments
Hardness, Mohs 1.0 - 2.0
1.0 - 2.0
Flexural Strength 27.6 MPa
4000 psi
Compressive Strength 62.1 MPa
9000 psi
Thermal Properties Metric English Comments
CTE, linear 6.30 µm/m-°C

@Temperature 20.0 °C
3.50 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 4.32 W/m-K
30.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1430 °C
2600 °F
Electrical Properties Metric English Comments
Dielectric Constant 5.5

@Frequency 1e+6 Hz
5.5

@Frequency 1e+6 Hz
Dielectric Strength 3.15 kV/mm
80.0 kV/in
Dissipation Factor 0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
Copyright © lookpolymers.com All Rights Reserved