Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia

Category Ceramic , Oxide , Magnesium Oxide , Potting/Casting Ceramic
Manufacturer Aremco
Trade Name Ceramacast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Ceramacast™ 584 High Temperature Potting & Casting Material Magnesia.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, quick-set ceramic for small parts.
Physical Properties Metric English Comments
Bulk Density 1.44 g/cc
0.0520 lb/in³
Powder
Porosity <= 6.00 %
<= 6.00 %
pH 11 - 12
11 - 12
Viscosity 18000 cP
18000 cP
Mechanical Properties Metric English Comments
Compressive Strength 31.0 MPa
4500 psi
Thermal Properties Metric English Comments
CTE, linear 11.7 µm/m-°C

@Temperature 20.0 °C
6.50 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 1540 °C
2800 °F
Shrinkage <= 4.00 %

@Temperature 538 °C
<= 4.00 %

@Temperature 1000 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
Dielectric Strength 3.94 kV/mm
100 kV/in
Processing Properties Metric English Comments
Dry Time >= 2 hour
>= 2 hour
Air dry
Cure Time 300 min
5.00 hour
2 hrs at 200°F; 3 hrs at 250°F
Pot Life <= 10.0 min
<= 10.0 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Acid Resistance Good
attacked by HF
Alkali Resistance Good
Color Off White
Mix Ratio 100:25-30
powder:liquid
Moisture Resistance Good