Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating

Category Ceramic , Polymer , Thermoset , Silicone
Manufacturer Aremco
Trade Name HiE-Coat™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body formulations designed to significantly improve the thermal efficiency of infrared heaters, furnaces, incinerators, and ovens used throughout the appliance, ceramics, chemical processing, metallurgical, and refining industries. Natural gas and oil savings in the range of 5–10% are typical using these coatings.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
Solids Content 42.5 %
42.5 %
by volume
57.1 %
57.1 %
by weight
Volatile Organic Compounds (VOC) Content 635 g/l
635 g/l
Viscosity 250 - 500 cP
250 - 500 cP
Thickness 25.4 microns
1.00 mil
recommended dry film thickness
61.0 microns
2.40 mil
estimated wet film thickness
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 593 °C
1100 °F
Flash Point 48.0 °C
118 °F
Processing Properties Metric English Comments
Processing Temperature 50.0 - 120 °C
122 - 248 °F
Application Temp
Cure Time 45.0 min

@Temperature 249 °C
0.750 hour

@Temperature 480 °F
preceeded by 1 hour air set
Shelf Life 6.00 Month

@Temperature 4.44 - 32.2 °C
6.00 Month

@Temperature 40.0 - 90.0 °F
Descriptive Properties Value Comments
Color Jet Black
Dry Film Coverage ft2/gal 681
at 1 mil
Thinner PM Acetate