Material Notes:
This grade offers a high level of fracture toughness for a zirconia material. Features include excellent fracture, corrosion, thermal shock, and wear resistance. Used for pump parts, valve components, bearings, and wear linings.
Physical Properties Metric English Comments
Specific Gravity 5.85 g/cc
5.85 g/cc
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Flexural Strength 414 MPa
60000 psi
Compressive Strength 1750 MPa
254000 psi
Thermal Properties Metric English Comments
CTE, linear 10.1 µm/m-°C
5.60 µin/in-°F
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1200 °C
2190 °F
Electrical Properties Metric English Comments
Dielectric Constant 28

@Frequency 1.00e+6 Hz
28

@Frequency 1.00e+6 Hz
Dielectric Strength 9.45 kV/mm
240 kV/in
Dielectric Loss Index 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz