Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95%

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Aremco
Trade Name Pyro-Paint™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Paint™ 634-ZO High Temperature Refractory Coating, ZO >95%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This highly-filled zirconium oxide-based coating produces a hard, chemically-resistant protective layer which is stable with aluminum, molybdenum, platinum, rhodium, and titanium. It is ideal for sealing porous ceramics and protecting other ceramic, graphite and metal structures up to 3270 °F. Exceptional for coating resistance wire heating elements in furnaces, protecting them from residue buildup which causes arcing and reduced element life.
Physical Properties Metric English Comments
Specific Gravity 2.02 g/cc
2.02 g/cc
Solids Content 35.5 %
35.5 %
volume
65 %
65 %
weight
pH 11 - 12
11 - 12
Coating pH
Viscosity 1000 - 2000 cP
1000 - 2000 cP
Storage Temperature 4.44 - 32.2 °C
40.0 - 90.0 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1800 °C
3270 °F
Processing Properties Metric English Comments
Processing Temperature 10.0 - 32.2 °C
50.0 - 90.0 °F
Application Temperature
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
>2 Hour Air Set Required Prior to Curing
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Color Tan
Coverage ft2/gal 570
Theoretical Coverage at 1 mil dry film thickness
Thinner 634 ZO-T
Weight/Gallon 23.5
Users viewing this material also viewed the following: