Material Notes:
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, good toughness, high melt point, good surface lubricity, and abrasion resistance. Vydyne 50BWFS maintains the chemical resistance typical of nylon to many chemicals, solvents, gasoline, and machine and motor oils. This resin is manufactured as an undried feedstock with a maximum moisture level of 0.5%. Vydyne 50BWFS permits the manufacturing of parts with good initial color plus good property and color retention when using regrind. This resin is recognized by Underwriters Laboratories and conforms to the requirements of many industrial, federal, and military specifications for premium-quality general purpose Nylon 66 resins. Typical Applications/End Uses. Vydyne 50BWFS has been successfully extruded in applications that do not require high melt strength, such as monofilament and bristle products.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Water Absorption 1.3 %
<br>@Time 86400 sec
1.3 %
<br>@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
50% RH; ISO 62
Linear Mold Shrinkage 0.012 cm/cm
<br>@Thickness 2.00 mm
0.012 in/in
<br>@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.014 cm/cm
<br>@Thickness 2.00 mm
0.014 in/in
<br>@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Break 45 %
45 %
ISO 527
Elongation at Yield 11 %
11 %
ISO 527
Tensile Modulus 3.00 GPa
435 ksi
ISO 527
Flexural Strength 33.0 MPa
4790 psi
ISO 178
Flexural Modulus 2.90 GPa
421 ksi
ISO 178
Poissons Ratio 0.40
0.40
ISO 527
Shear Modulus 1.07 GPa
155 ksi
Calculated
Izod Impact, Notched (ISO) 5.50 kJ/m²
2.62 ft-lb/in²
ISO 180
Charpy Impact Unnotched NB
<br>@Temperature 23.0 °C
NB
<br>@Temperature 73.4 °F
ISO 179
NB
<br>@Temperature -30.0 °C
NB
<br>@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.550 J/cm²
<br>@Temperature -30.0 °C
2.62 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179
0.650 J/cm²
<br>@Temperature 23.0 °C
3.09 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear 11.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
6.11 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359
CTE, linear, Transverse to Flow 12.0 µm/m-°C
<br>@Thickness 2.00 mm,<br> Temperature 23.0 - 55.0 °C
6.67 µin/in-°F
<br>@Thickness 0.0787 in,<br> Temperature 73.4 - 131 °F
ISO 11359
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ISO 75
Vicat Softening Point 237 °C
<br>@Load 5.10 kg
459 °F
<br>@Load 11.2 lb
ISO 306
UL RTI, Electrical 65.0 °C
<br>@Thickness 0.400 mm
149 °F
<br>@Thickness 0.0157 in
UL 746B
130 °C
<br>@Thickness 0.710 mm
266 °F
<br>@Thickness 0.0280 in
UL 746B
130 °C
<br>@Thickness 1.50 mm
266 °F
<br>@Thickness 0.0591 in
UL 746B
130 °C
<br>@Thickness 3.00 mm
266 °F
<br>@Thickness 0.118 in
UL 746B
UL RTI, Mechanical with Impact 65.0 °C
<br>@Thickness 0.400 mm
149 °F
<br>@Thickness 0.0157 in
UL 746B
75.0 °C
<br>@Thickness 0.710 mm
167 °F
<br>@Thickness 0.0280 in
UL 746B
75.0 °C
<br>@Thickness 1.50 mm
167 °F
<br>@Thickness 0.0591 in
UL 746B
75.0 °C
<br>@Thickness 3.00 mm
167 °F
<br>@Thickness 0.118 in
UL 746B
UL RTI, Mechanical without Impact 65.0 °C
<br>@Thickness 0.400 mm
149 °F
<br>@Thickness 0.0157 in
UL 746B
85.0 °C
<br>@Thickness 0.710 mm
185 °F
<br>@Thickness 0.0280 in
UL 746B
85.0 °C
<br>@Thickness 1.50 mm
185 °F
<br>@Thickness 0.0591 in
UL 746B
85.0 °C
<br>@Thickness 3.00 mm
185 °F
<br>@Thickness 0.118 in
UL 746B
Flammability, UL94 V-2
<br>@Thickness 0.400 mm
V-2
<br>@Thickness 0.0157 in
V-2
<br>@Thickness 0.710 mm
V-2
<br>@Thickness 0.0280 in
V-2
<br>@Thickness 1.50 mm
V-2
<br>@Thickness 0.0591 in
V-2
<br>@Thickness 3.00 mm
V-2
<br>@Thickness 0.118 in
Oxygen Index 27 %
27 %
ASTM D2863
Glow Wire Test 725 °C
<br>@Thickness 0.710 mm
1340 °F
<br>@Thickness 0.0280 in
Ignition Temperature; IEC 60695-2-12
725 °C
<br>@Thickness 1.50 mm
1340 °F
<br>@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-12
725 °C
<br>@Thickness 3.00 mm
1340 °F
<br>@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-12
825 °C
<br>@Thickness 0.710 mm
1520 °F
<br>@Thickness 0.0280 in
Flame Index; IEC 60695-2-12
825 °C
<br>@Thickness 1.50 mm
1520 °F
<br>@Thickness 0.0591 in
Flame Index; IEC 60695-2-12
960 °C
<br>@Thickness 3.00 mm
1760 °F
<br>@Thickness 0.118 in
Flame Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+15 ohm-cm
<br>@Thickness 3.00 mm
6.00e+15 ohm-cm
<br>@Thickness 0.118 in
IEC 60093
Dielectric Strength 12.0 kV/mm
<br>@Thickness 3.00 mm
305 kV/in
<br>@Thickness 0.118 in
IEC 60243
Arc Resistance 120 - 180 sec
<br>@Thickness 3.00 mm
120 - 180 sec
<br>@Thickness 0.118 in
UL 746A
Comparative Tracking Index >= 600 V
<br>@Thickness 3.00 mm
>= 600 V
<br>@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec
<br>@Thickness 0.710 mm
7.0 - 15 sec
<br>@Thickness 0.0280 in
UL 746B
15 - 30 sec
<br>@Thickness 1.50 mm
15 - 30 sec
<br>@Thickness 0.0591 in
UL 746B
30 - 60 sec
<br>@Thickness 3.00 mm
30 - 60 sec
<br>@Thickness 0.118 in
UL 746B
High Amp Arc Ignition, HAI >= 120 arcs
<br>@Thickness 0.710 mm
>= 120 arcs
<br>@Thickness 0.0280 in
UL 746A
>= 120 arcs
<br>@Thickness 1.50 mm
>= 120 arcs
<br>@Thickness 0.0591 in
UL 746A
>= 120 arcs
<br>@Thickness 3.00 mm
>= 120 arcs
<br>@Thickness 0.118 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
<br>@Thickness 3.00 mm
0.000 - 0.394 in/min
<br>@Thickness 0.118 in
UL 746A
Processing Properties Metric English Comments
Processing Temperature 270 - 310 °C
518 - 590 °F
Melt Temperature 275 - 305 °C
527 - 581 °F
Mold Temperature 15.0 - 95.0 °C
59.0 - 203 °F
Injection Pressure 55.0 - 140 MPa
7980 - 20300 psi
Hold Pressure 55.0 - 140 MPa
7980 - 20300 psi
Back Pressure 0.200 - 1.00 MPa
29.0 - 145 psi
Clamp Pressure 29.43 - 68.67 MPa
4268 - 9960 psi
Copyright © lookpolymers.com All Rights Reserved