Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Hot Wire Ignition, HWI = 30 sec Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 0.851 mm
15 - 30 sec

@Thickness 0.0335 in
UL 746
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10FRN (V) 15 MFI, 5VA, Flame Retardant, UV Stabilized Polycarbonate With Release
ROHS Compliant.Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10R-(V18) 18 MFI UV Stabilized Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 1.50 mm
15 - 30 sec

@Thickness 0.0591 in
PLC 3
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical ALPHALAC SG910 HIPS
High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electric appliancesCA..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical HIPS 403AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical LI911 ASA
Description: Good Weatherability, High FlowApplication: Air-conditioner grill, Sawing Machine Cover, Electric/Electronic ApplicationsCAS: 26299-47-8Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical LI942 Heat Resistant ASA
Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=0.750 mm
15 - 30 sec

@Thickness >=0.0295 in
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUMID GP2330B(W) PA66+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Air Intake Manifold, Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose
Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.30 mm
15 - 30 sec

@Thickness >=0.130 in
LG Chemical Lupox® GP1000D PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.30 mm
15 - 30 sec

@Thickness >=0.130 in
LG Chemical Lupox® GP1000SB PBT
Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical Lupox® GP2056F PBT+GF5%
Description: Injection Molding, PBT+GF5%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical AF360 ABS, TBBA-free Flame Retardant
Feature: Injection Molding, TBBA-free Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 84852-53-9 and 1309-64-4Information provided b..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=2.00 mm
15 - 30 sec

@Thickness >=0.0787 in
LG Chemical LUPOL GP3156F Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided ..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=0.710 mm
15 - 30 sec

@Thickness >=0.0280 in
LG Chemical Lupox® GP2156FT PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
LG Chemical XR401 ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (lamp housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 ..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness 3.00 mm
15 - 30 sec

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
Hot Wire Ignition, HWI 15 - 30 sec

@Thickness >=1.50 mm
15 - 30 sec

@Thickness >=0.0591 in
LG Chemical HF350U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved