Polymer Property : Linear Mold Shrinkage, Transverse = 0.014 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ASTM D955
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin
NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
STN EN ISO 294-4
Plastcom PLASTALEN® PC 69 T 10 003/1M Polypropylene reinforced with mineral filler
Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o.
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Thickness 3.17 mm
0.014 - 0.016 in/in

@Thickness 0.125 in
ASTM D955
Network Polymers Softflex® 7210 Black
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Euronil
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6
Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
DAM; ISO 294-4
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66  (Unverified Data**)
Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin
Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
60x60x2; 260°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Pocan® DP 7102 000000 PBT, 32% Mineral
PBT, 32% mineral, injection molding, LDSInformation provided by LANXESS.
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant
Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Solvay TECHNYL® B 216 Natural D PA66/6, DRY
Description: Unreinforced copolyamide 66/6, medium viscosity, for injection molding.Available in: EuropeProduct Applications: TECHNYL B 216 offers an excellent combination between impact resistance,..
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Time 86400 sec
0.014 - 0.016 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRILOY UA200A PPA (Asia Pacific)
LNP LUBRILOY* UA200A is a compound based on Polyphthalamide resin containing Aramid Fiber, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm

@Time 86400 sec
0.014 - 0.016 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT
4.2 specific gravity, PBT, gray
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp P1000P PA 6
LNP* Thermocomp* P1000P is a compound based on Nylon 6 resin. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
TPE Method
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
24 hours
Teknor Apex TEKRON® 4300LM-P96-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO DIS 294-4
Wellman Wellamid® T-731E-BK 10% Reinforced Abrasion Resistant Nylon 6
Description: Abrasion Resistant Nylon 6Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.014 - 0.017 cm/cm
0.014 - 0.017 in/in
ISO DIS 294-4
Wellman Wellamid® WE1359 25% Glass Sphere Filled, Toughened Nylon 66
Description: Glass Sphere Filled, Toughened Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ISO DIS 294-4
Wellman Wellamid® WE1410 43% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® BZ 1/2 PA6
Product description: Grilon BZ 1/2 is an unreinforced, impact modified PA6 injection molding grade with normal melt viscosity. Grilon BZ 1/2 has the following important properties: Good flow behavio..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4, 2577
EMS-Grivory Grivory® L 25 NZ ESD PA12
Product Description: Grilamid L 25 NZ ESD is a high viscosity, anti-static extrusion grade of Polyamide 12 (PA12). Grilamid L 25 NZ ESD is impact modified and heat stabilized. The inherent color of ..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 100ST BK602 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST BK602 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
DAM; ISO 294-4 2577
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Eurotec
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural
Information provided by Eurotec®
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.014 in/in

@Thickness 0.157 in,
Time 24.0 hour
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 4.00 mm,
Time 86400 sec
0.014 in/in

@Thickness 0.157 in,
Time 24.0 hour
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-27 GF30 I Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai..
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Diameter 2.00 mm
0.014 in/in

@Diameter 0.0787 in
ISO 294-4
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM
Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4
Azoty Tarnow™ Tarnamid® T-27 MF30 Polyamide 6 - Mineral Reinforced
30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani..
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
ISO 294-4 2577
DuPont Performance Polymers Sorona® 3301V NC010 Polytrimethylene Terephthalate (PTT)
Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301V NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight develo..