| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics Cycolac® INP222 ABS Bulk MMASAN. Provides an economical option for achieving greater melt strength in polymers. |
|||
| Flexural Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
ISO 178 |
| Polykemi AB POLYfill PPHC T5040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| PolyOne Nymax™ 1200 IL Natural Polyamide 66 (Nylon 66) The Nymax® 1200 IL is an internally lubricated, unfilled nylon 6/6 designed for exceptional processing and mold release. This grade is intended primarily for injection molded applications where a g.. |
|||
| Flexural Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
ISO 178 |
| DuPont Performance Polymers Delrin® FG500P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500P is a medium viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information p.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Techmer ES HiFill® PA6/6 E4 A1 Nylon 66 Availability: North AmericaForms: PelletsFeatures: High ViscosityInformation provided by TP Composites, Inc. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Europe-Africa-Middle East) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Techmer ES HiFill® PA6/6 NAT Availability: North AmericaForms: PelletsAppearance: Natural ColorTPCI# 8384101Information provided by TP Composites, Inc. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Techmer ES Plastiblend® PA6 NAT001 Nylon 6 Availability: North AmericaForms: PelletsFeatures: Good Processability and High FlowAppearance: NaturalTPCI# 1327102Information provided by TP Composites, Inc. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Techmer ES HiFill® PBT 0150 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Westlake Plastics Polyethersulfone High resistance to heat and combustibility, low smoke emission, and transparency are the combination of properties possessed by stock shapes extruded from PES. These, coupled with light weight, good.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM-D790 |
| Polyram RamOfin PPC365T8 Polypropylene, 40% Mineral Filled 40% mineral filled, heat stabilized polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D790 |
| Ensinger Delrin® 150 Homopolymer Acetal (POM) Ensinger's Delrin® 150 stock shapes are a homopolymer acetal manufactured using DuPont Delrin 150 Resin. It is a crystalline plastic which offers an excellent balance of properties to bridge the g.. |
|||
| Flexural Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
ISO 178 |
| DuPont Performance Polymers Delrin® 500PE NC010A Acetal Homopolymer Delrin® 500PE NC010A is a medium viscosity acetal homopolymer, an enhanced version of Delrin® 500P with extremely low VOC emissions. It has improved processing thermal stability, and good mechanic.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| Ecomass® 705ZD70 Tungsten Filled ABS Nontoxic Alternative to Lead (Pb) for radiation shielding applicationsHigh specific GravityTungsten Filled ABS compoundRigidGood ToughnessInformation provided by Technical Polymers |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 50%RH; ISO 178 |
| DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
| Flexural Modulus | 2.90 GPa | 420 ksi | ASTM D-790 |
| Axiall HR-5009 Rigid PVC, Molding Georgia Gulf HR-5009 is a rigid, fitting-grade PVC compound designed for hot runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, which incl.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
| Cast Nylons Nycast® Nyloil®-FG Lubricated Nylon, Food Grade NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
| Ashley Polymers Ashlene® RH190-PF Acetal, PTFE Filled A wear-resistant grade homopolymer resin with 1.5% PTFE.Data provided by the manufacturer |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ASTM D790 |
| Adell AS-30 Nylon 66, General Purpose Data provided by Adell Plastics, Inc. |
|||
| Flexural Modulus | 2.90 GPa @Temperature 23.0 °C |
421 ksi @Temperature 73.4 °F |
ISO 178 |
| DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | ISO 178 |
| Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To.. |
|||
| Flexural Modulus | 2.90 GPa | 421 ksi | 2 mm/min; ISO 178 |
| Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat.. |
|||