Polymer Property : UL RTI, Electrical = 266 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® CE15315 NC010 PBT  (Unverified Data**)
Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® S600F40 BK851 PBT  (Unverified Data**)
Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® SK603 BK851 PBT  (Unverified Data**)
Crastin® SK603 BK851 is a 20% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 6.00 mm
266 °F

@Thickness 0.236 in
UL 746B
DuPont Performance Polymers Crastin® SK605 BK851 PBT  (Unverified Data**)
Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness >=1.50 mm
266 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2076F PBT+GF7%
Description: Injection Molding, PBT+GF7%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Electrical 130 °C

@Thickness >=1.50 mm
266 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2156FL PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by..
UL RTI, Electrical 130 °C

@Thickness >=2.00 mm
266 °F

@Thickness >=0.0787 in
LG Chemical Lupoy NF1009F 15 Polycarbonate Resin
Description: LUPOY NF 1009F15, eco-friendly UL94 V0/2.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpare..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® 18 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL746B
Mitsubishi Xantar® 27 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® FC 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G2F 23 R Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness >=3.00 mm
266 °F

@Thickness >=0.118 in
LG Chemical LUPOY GP1000MR PC, Transparent
Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..
UL RTI, Electrical 130 °C

@Thickness 0.710 mm
266 °F

@Thickness 0.0280 in
UL 746
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM
Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive:LubricantNucleating Agent Features: Fast Molding CycleGeneral PurposeGood Mold ReleaseGood StiffnessHigh RigidityLubricatedNucleatedUses:Bearings..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746B
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL746B
DSM Arnite® T08 200 (extrusion) T08 200 PBT (European and Asian Grade)  (discontinued **)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL746B
Mitsubishi Xantar® F 22 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher..