Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.14 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
23/23°C; ASTM D792
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black
Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.14 g/cc
1.14 g/cc
23/23°C; ASTM D792
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Polymax® Maxelast® P2735 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
S&E Specialty Polymers GF-1831 PVC
Description: High grade oil resistant PVC/Nitril soling material with excellent abrasion and slip resistant properties designed for work boot applicationsInformation provided by S&E Specialty Polyme..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific)
PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D 792
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East)
PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D1505
Honeywell Aegis™ HFX High Barrier Nylon  (discontinued **)
Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is ..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
LG Chemical LUMID GN1001BF PA66, Halogen Free Flame Retardant
Feature: Injection Molding, PA66, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4 and 37640-57-6Information provided by LG Chemical
Specific Gravity 1.14 g/cc
1.14 g/cc
Lehigh Technologies 140 Mesh Ground Reclaimed Whole Tire Rubber
A free flowing black powder produced from vulcanized rubber materialInformation provided by Lehigh Technologies, LLC.
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
SABIC Innovative Plastics LNP STAT-KON AE004 ABS
LNP STAT-KON* AE004 is a compound based on ABS resin containing 20% Carbon Fiber. Added feature of this material is: Electrically Conductive.
Specific Gravity 1.14 g/cc
1.14 g/cc
Spartech 114-4-62 PVC and Alloy Products for Footwear
Used for waterproof boots.Information provided by Spartech
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Samsung Cheil Industries Infino® WP-1089 PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
Specific Gravity 1.14 g/cc
1.14 g/cc
23°C; ASTM D792
Teknor Apex APEX® 3200-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Teknor Apex Monprene® MP-2780 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Chase Plastics CP Pryme® NN200L (DAM) Nylon 66, Internally Lubricated
Information provided by Chase Plastics.
Specific Gravity 1.14 g/cc
1.14 g/cc
Absolute Drying; ASTM-D792
Toyobo GLAMIDE® T-803 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Specific Gravity 1.14 g/cc
1.14 g/cc
Absolute Drying; ASTM-D792
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Specific Gravity 1.14 g/cc
1.14 g/cc
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Atomite Whiting Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Specific Gravity 1.14 g/cc
<br>@Temperature 25.0 °C
1.14 g/cc
<br>@Temperature 77.0 °F
Dow Corning SILASTIC® 9280/60E KIT PARTS A&B
75 Shore A hardness, two-part, 1 to 1 mix, translucent, injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning
Specific Gravity 1.14 g/cc
1.14 g/cc
DIN 53 479
Hippe PA 66 Nylon 66
The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec..
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi..
Specific Gravity 1.14 - 1.20 g/cc
1.14 - 1.20 g/cc
ASTM D792
Buckeye Polymers BP FLEX D6509 CU BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Ascend Performance Materials Vydyne® 66R Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66R resin offers high strength, ..
Specific Gravity 1.14 g/cc
1.14 g/cc
Radici Radilon® A 35E 990 (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Specific Gravity 1.14 g/cc
1.14 g/cc
Mixed; TM R050-16
Resinlab® EP1026 Clear Epoxy Adhesive
Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
LG Chemical LUPOY NS5000C PC/ABS, High Impact
Description: Injection Molding, PC/ABS, Heat Resistance, High Flow, High ImpactApplication: Automotive (Interior)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical
Copyright © lookpolymers.com All Rights Reserved