| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | |
|
Polykemi AB POLYfill PPH 150DNH Polypropylene Homopolymer, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **)
Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Primef® 7010 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **)
Primef 7010 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers improved mechanical properties versus Primef 7002 (also 65% mineral/glass fiber), but with less flu..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa FW-650 Flame Retardant ABS
Features:Weather resistanceSuper high impact resistanceApplications:Injection moldingSwitchSocketInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Back Pressure | 0.400 - 1.00 MPa | 58.0 - 145 psi | |
|
Kingfa JH720 G10D 10% Glass Fiber Reinforced PC
Features:Good processing propertiesLow tendency to warpHigh mechanical strengthGood size stabilityGood surfaceSuitable for exact moldingApplications:Exact mechanism partsPrinter, photocopies, scanne..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa JH720 G50 50% Glass Fiber Reinforced PC
Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p..
|
|||
| Back Pressure | 0.700 - 1.00 MPa | 102 - 145 psi | |
|
Kingfa JH820 Modified PC
Features:Excellent balance propertiesSuper high impact strengthHigh stiffnessGood size stabilityGood surface, high glossHigh transparencyApplications:Injection moldingHousehold applianceBusiness mac..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa JH950-402 Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surfaceApplications:Small household appliance cabinetControllerSocketShell of a..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa JH710 G20 Flame Retardant & 20% Glass Fiber Reinforced PC
Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:CD-ROM, DVDPrinter, photocopier cabinetSc..
|
|||
| Back Pressure | 0.700 - 1.00 MPa | 102 - 145 psi | |
|
Kingfa MAC-601 AC PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection molding |
|
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem 475-860N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem AB760LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-860 TPE Compound
Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-975B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem LP-830 TPE Compound
This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem LP-870 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
|
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | |
|
Polykemi AB POLYfill PP 150ENH Polypropylene, Flame Retardant, Halogen Free
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.200 - 1.00 MPa | 29.0 - 145 psi | |
|
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, at Equilibrium (65% RH)
The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
|
|||