| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.02 - 1.67 g/cc | 0.0368 - 0.0603 lb/in³ | Average value: 1.20 g/cc Grade Count:126 |
| 1.03 - 1.03 g/cc <br>@Temperature 290 - 290 °C |
0.0372 - 0.0372 lb/in³ <br>@Temperature 554 - 554 °F |
Average value: 1.03 g/cc Grade Count:1 | |
| Water Absorption | 0.0500 - 9.00 % | 0.0500 - 9.00 % | Average value: 2.15 % Grade Count:82 |
| Moisture Absorption at Equilibrium | 0.170 - 3.10 % | 0.170 - 3.10 % | Average value: 2.06 % Grade Count:32 |
| Water Absorption at Saturation | 6.50 - 9.00 % | 6.50 - 9.00 % | Average value: 8.01 % Grade Count:11 |
| Viscosity Test | 150 - 205 cm³/g | 150 - 205 cm³/g | Average value: 178 cm³/g Grade Count:4 |
| Linear Mold Shrinkage | 0.00100 - 0.0280 cm/cm | 0.00100 - 0.0280 in/in | Average value: 0.0135 cm/cm Grade Count:111 |
| Linear Mold Shrinkage, Transverse | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.0127 cm/cm Grade Count:19 |
| Melt Flow | 4.00 - 130 g/10 min | 4.00 - 130 g/10 min | Average value: 49.8 g/10 min Grade Count:7 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 55.0 - 88.0 | 55.0 - 88.0 | Average value: 77.3 Grade Count:11 |
| Hardness, Rockwell R | 90.0 - 125 | 90.0 - 125 | Average value: 116 Grade Count:44 |
| Ball Indentation Hardness | 110 - 150 MPa | 16000 - 21800 psi | Average value: 129 MPa Grade Count:9 |
| Tensile Strength, Ultimate | 4.00 - 137 MPa | 580 - 19900 psi | Average value: 70.9 MPa Grade Count:73 |
| 24.0 - 116 MPa <br>@Temperature -40.0 - 80.0 °C |
3480 - 16800 psi <br>@Temperature -40.0 - 176 °F |
Average value: 49.1 MPa Grade Count:6 | |
| 10.0 - 95.0 MPa <br>@Temperature -20.0 - 100 °C |
1450 - 13800 psi <br>@Temperature -4.00 - 212 °F |
Average value: 49.1 MPa Grade Count:1 | |
| 10.0 - 95.0 MPa <br>@Strain 1.00 - 3.00 % |
1450 - 13800 psi <br>@Strain 1.00 - 3.00 % |
Average value: 49.1 MPa Grade Count:1 | |
| Tensile Strength, Yield | 34.5 - 193 MPa | 5000 - 28000 psi | Average value: 72.6 MPa Grade Count:65 |
| 62.0 - 107 MPa <br>@Temperature -40.0 - 77.0 °C |
8990 - 15500 psi <br>@Temperature -40.0 - 171 °F |
Average value: 84.5 MPa Grade Count:1 | |
| Elongation at Break | 2.20 - 300 % | 2.20 - 300 % | Average value: 33.9 % Grade Count:104 |
| 20.0 - 300 % <br>@Temperature -40.0 - 150 °C |
20.0 - 300 % <br>@Temperature -40.0 - 302 °F |
Average value: 97.5 % Grade Count:5 | |
| Elongation at Yield | 2.00 - 25.0 % | 2.00 - 25.0 % | Average value: 11.0 % Grade Count:42 |
| 5.00 - 30.0 % <br>@Temperature -40.0 - 77.0 °C |
5.00 - 30.0 % <br>@Temperature -40.0 - 171 °F |
Average value: 17.5 % Grade Count:1 | |
| Modulus of Elasticity | 1.10 - 12.4 GPa | 160 - 1800 ksi | Average value: 3.02 GPa Grade Count:64 |
| 0.400 - 3.50 GPa <br>@Temperature 40.0 - 150 °C |
58.0 - 508 ksi <br>@Temperature 104 - 302 °F |
Average value: 1.37 GPa Grade Count:5 | |
| Flexural Yield Strength | 39.0 - 276 MPa | 5660 - 40000 psi | Average value: 101 MPa Grade Count:94 |
| 38.0 - 140 MPa <br>@Temperature -40.0 - 80.0 °C |
5510 - 20300 psi <br>@Temperature -40.0 - 176 °F |
Average value: 86.8 MPa Grade Count:2 | |
| Flexural Modulus | 0.255 - 12.4 GPa | 37.0 - 1800 ksi | Average value: 2.85 GPa Grade Count:99 |
| 0.400 - 4.30 GPa <br>@Temperature -40.0 - 80.0 °C |
58.0 - 624 ksi <br>@Temperature -40.0 - 176 °F |
Average value: 2.14 GPa Grade Count:2 | |
| Compressive Yield Strength | 34.0 - 97.0 MPa | 4930 - 14100 psi | Average value: 79.5 MPa Grade Count:4 |
| Shear Strength | 56.0 - 69.0 MPa | 8120 - 10000 psi | Average value: 63.0 MPa Grade Count:6 |
| Izod Impact, Notched | 0.290 - 7.47 J/cm | 0.543 - 14.0 ft-lb/in | Average value: 0.937 J/cm Grade Count:73 |
| 0.350 - 1.38814 J/cm <br>@Temperature -40.0 - -40.0 °C |
0.656 - 2.60056 ft-lb/in <br>@Temperature -40.0 - -40.0 °F |
Average value: 0.642 J/cm Grade Count:4 | |
| 0.300 - 0.427 J/cm <br>@Temperature -40.0 - -40.0 °C |
0.562 - 0.800 ft-lb/in <br>@Temperature -40.0 - -40.0 °F |
Average value: 0.642 J/cm Grade Count:2 | |
| 0.300 - 0.427 J/cm <br>@Thickness 1.57 - 3.17 mm |
0.562 - 0.800 ft-lb/in <br>@Thickness 0.0618 - 0.125 in |
Average value: 0.642 J/cm Grade Count:2 | |
| Izod Impact, Unnotched | 5.34 J/cm - NB | 10.0 ft-lb/in - NB | Average value: 6.71 J/cm Grade Count:7 |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² - NB | 1.43 ft-lb/in² - NB | Average value: 5.85 kJ/m² Grade Count:21 |
| 3.00 - 6.00 kJ/m² <br>@Temperature -40.0 - -20.0 °C |
1.43 - 2.86 ft-lb/in² <br>@Temperature -40.0 - -4.00 °F |
Average value: 4.00 kJ/m² Grade Count:5 | |
| Izod Impact, Unnotched (ISO) | 45.0 - 60.0 kJ/m² <br>@Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² <br>@Temperature -22.0 - -22.0 °F |
Average value: 53.8 kJ/m² Grade Count:2 |
| Charpy Impact Unnotched | 3.00 J/cm² - NB | 14.3 ft-lb/in² - NB | Average value: 6.80 J/cm² Grade Count:39 |
| 2.00 J/cm² - NB <br>@Temperature -40.0 - -20.0 °C |
9.52 ft-lb/in² - NB <br>@Temperature -40.0 - -4.00 °F |
Average value: 6.01 J/cm² Grade Count:17 | |
| Charpy Impact, Notched | 0.150 J/cm² - NB | 0.714 ft-lb/in² - NB | Average value: 0.663 J/cm² Grade Count:40 |
| 0.150 J/cm² - NB <br>@Temperature -40.0 - -20.0 °C |
0.714 ft-lb/in² - NB <br>@Temperature -40.0 - -4.00 °F |
Average value: 0.311 J/cm² Grade Count:15 | |
| Tensile Creep Modulus, 1000 hours | 700 MPa | 102000 psi | Average value: 700 MPa Grade Count:3 |
| Taber Abrasion, mg/1000 Cycles | 5.00 - 24.0 | 5.00 - 24.0 | Average value: 10.4 Grade Count:5 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.0 - 100 µm/m-°C | 5.56 - 55.6 µin/in-°F | Average value: 70.9 µm/m-°C Grade Count:42 |
| CTE, linear, Transverse to Flow | 10.0 - 85.0 µm/m-°C | 5.56 - 47.2 µin/in-°F | Average value: 64.0 µm/m-°C Grade Count:5 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 4.11e+16 ohm-cm Grade Count:70 |
| Surface Resistance | 100 - 1.00e+16 ohm | 100 - 1.00e+16 ohm | Average value: 5.18e+14 ohm Grade Count:35 |
| Dielectric Constant | 2.70 - 8.00 | 2.70 - 8.00 | Average value: 3.88 Grade Count:29 |
| Dielectric Strength | 13.0 - 70.0 kV/mm | 330 - 1780 kV/in | Average value: 26.1 kV/mm Grade Count:52 |
| Dissipation Factor | 0.00500 - 0.200 | 0.00500 - 0.200 | Average value: 0.0429 Grade Count:19 |
| Dielectric Loss Index | 0.0200 - 0.300 | 0.0200 - 0.300 | Average value: 0.128 Grade Count:6 |
| Arc Resistance | 60.0 - 179 sec | 60.0 - 179 sec | Average value: 121 sec Grade Count:9 |
| Comparative Tracking Index | 225 - 600 V | 225 - 600 V | Average value: 557 V Grade Count:48 |