Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Electrical = 65.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources NY66-GP1 General Purpose Nylon 66
General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized
General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-FRG10 Modified-PPO, V-1 Flame Retardant, 10% Glass Reinforced
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 10% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Modified-Polyphenylene Oxide, Structural Foam Grade, Easy FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechani..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL 746
Polymer Resources NY66-IM2 Impact Modified Nylon 66
Nylon 66, Superior Impact Modified, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are ..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6  (Unverified Data**)
Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 65.0 °C

@Thickness >=3.00 mm
149 °F

@Thickness >=0.118 in
LG Chemical LUMID GN-2251BF Flame Retardant PA Alloy
Feature: Injection Molding, Flame Retardant PA AlloyApplication: E&E partsInformation provided by LG Chemical
UL RTI, Electrical 65.0 °C

@Thickness 0.810 mm
149 °F

@Thickness 0.0319 in
UL 746
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K222-KGMV14 Nylon 6-25% Glass and Mineral Reinforced (European Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K224-G0 Nylon 6-50% Glass Reinforced (European Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
UL746B
DSM Akulon® K224-G6 Nylon 6-30% Glass Reinforced (European and Asian Grade) (Dry)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide AG10K PA66, 50% Glass Filled, Injection Molded
AG10 is a Heat and Hydrolytically Stabilized, 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide AG4K PA66, 20% Glass Filled, Injection Molded
AG4K is a Heat and Hydrolytically Stabilized, 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppl..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide AST03 PA66, Impact Modified, Injection Molded
AST03 is an Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded
BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide BG10 PA6, 50% Glass Filled, Injection Molded
BG10 is a 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BG10H PA6, 50% Glass Filled, Injection Molded
BG10 is a Heat Stabilized, 50% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded
BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide BST01 PA6, Impact Modified, Injection Molded
BST01 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
UL746B
DSM Akulon® K224-G0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K224-G3 (Cond.) 15% Glass Reinforced Nylon 6 (North America)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide AG7 PA66, 35% Glass Filled, Injection Molded
AG7 is a 35% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded
BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 0.750 mm
149 °F

@Thickness 0.0295 in
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded
BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
UL RTI, Electrical 65.0 °C

@Thickness 0.400 mm
149 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM
Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr..
UL RTI, Electrical 65.0 °C

@Thickness 1.50 mm
149 °F

@Thickness 0.0591 in
UL746B
DSM Akulon® K224-TG9 Nylon 6-45% Glass Reinforced (European and Asian Grade) (Cond)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
UL RTI, Electrical 65.0 °C

@Thickness 3.00 mm
149 °F

@Thickness 0.118 in
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded
BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Copyright © lookpolymers.com All Rights Reserved