Polymer Property : UL RTI, Electrical = 130 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Electrical 130 °C

@Thickness 0.800 mm
266 °F

@Thickness 0.0315 in
UL 746
Polymer Resources TP-FRG15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant
Polybutylene Terephthalate, 15% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® CE15315 NC010 PBT  (Unverified Data**)
Crastin® CE15315 NC010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Crastin® LW9320 BK851 PBT  (Unverified Data**)
Crastin® LW9320 BK851 is a 20% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Crastin® S600F20 BK851 PBT  (Unverified Data**)
Crastin® S600F20 BK851 is an unreinforced, lubricated, medium viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746B
DuPont Performance Polymers Crastin® S600F40 NC010 PBT  (Unverified Data**)
Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® SK601 BK851 PBT  (Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746B
DuPont Performance Polymers Crastin® SK605 BK851 PBT  (Unverified Data**)
Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746B
DuPont Performance Polymers Crastin® SK605 BK851 PBT  (Unverified Data**)
Crastin® SK605 BK851 is a 30% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 0.710 mm
266 °F

@Thickness 0.0280 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66  (Unverified Data**)
Zytel® 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness >=3.00 mm
266 °F

@Thickness >=0.118 in
LG Chemical Lupoy NF1007F 10R Polycarbonate Resin
Description: LUPOY NF 1007F10R, eco-friendly UL94 V0/3.0 mm, is designed for extrusion and injection molding products. It combines an excellent physical property balance of heat resistance, transpar..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL746B
Mitsubishi Xantar® 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® 27 U Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL746B
Mitsubishi Xantar® G4F 23 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
UL RTI, Electrical 130 °C

@Thickness >=1.50 mm
266 °F

@Thickness >=0.0591 in
LG Chemical Lupox® GP2156FM PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Electrical 130 °C

@Thickness >=3.00 mm
266 °F

@Thickness >=0.118 in
LG Chemical Lupox® GP2156FM PBT+GF15%
Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical
UL RTI, Electrical 130 °C

@Thickness 0.800 mm
266 °F

@Thickness 0.0315 in
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® T06 200 PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® TV4 230 SF PBT-15% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded
Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer..
UL RTI, Electrical 130 °C

@Thickness 0.400 mm
266 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
UL RTI, Electrical 130 °C

@Thickness 0.750 mm
266 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
UL RTI, Electrical 130 °C

@Thickness 3.00 mm
266 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
UL 746B
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM
Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters..
UL RTI, Electrical 130 °C

@Thickness 6.00 mm
266 °F

@Thickness 0.236 in
UL 746B
DuPont Performance Polymers Crastin® LW9030 BK851 PBT  (Unverified Data**)
Crastin® LW9030 BK851 is a 30% glass fiber reinforced, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warp..
UL RTI, Electrical 130 °C

@Thickness >=3.00 mm
266 °F

@Thickness >=0.118 in
LG Chemical LUPOY GP1000ML PC, Transparent
Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical