Polymer Property : UL RTI, Mechanical with Impact = 167 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.710 mm
167 °F

@Thickness 0.0280 in
DAM; UL 746B
DuPont Performance Polymers Zytel® 101L BKB009 Nylon 66  (Unverified Data**)
Zytel® 101L BKB009 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
UL RTI, Mechanical with Impact 75.0 °C

@Thickness >=2.00 mm
167 °F

@Thickness >=0.0787 in
LG Chemical AF312A ABS, Flame Retardant
Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
DAM
Aardvark Polymers Aarlon® 4055FR PA 6/6 Rotational Molding Resin
Aarlon 4055FR is a premium flame retardant type 6/6 nylon.Aarlon 4055FR is halogen, heavy metal, and red phosphorus free.Aarlon 4055FR is UL94 V-0 rated.Aarlon 4055FR is semi-crystalline, nucleated,..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0590 in
UL 746
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
DAM; UL 746B
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
Eurostar Starflam P10002E PA6, Injection Molded
Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.60 mm
167 °F

@Thickness 0.0630 in
Eurostar Starflam R10002E PA66/6, Injection Molded
Starflam R10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 66/Polyamide 6 Injection Molding Resin (also known as R1000Z220EM)Information provided by Polymer Te..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.400 mm
167 °F

@Thickness 0.0157 in
UL 746
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.710 mm
167 °F

@Thickness 0.0280 in
UL 746
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.710 mm
167 °F

@Thickness 0.0280 in
UL 746
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 21SPG1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth America Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood ToughnessHigh Rigidit..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM
Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM
Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746B
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.710 mm
167 °F

@Thickness 0.0280 in
UL 746B
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.710 mm
167 °F

@Thickness 0.0280 in
UL 746
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL 746
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.750 mm
167 °F

@Thickness 0.0295 in
UL746B
DSM Arnite® T06 204 SN PBT (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 1.50 mm
167 °F

@Thickness 0.0591 in
UL 746
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 3.00 mm
167 °F

@Thickness 0.118 in
UL 746
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..