Electrical Properties Metric English Comments
Arc Resistance 120 - 180 sec
120 - 180 sec
UL-746A rating 5 (120-180 sec)
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade  (disco
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha..
Arc Resistance 120 sec
120 sec
ASTM D495
Kolon KOPET® KP133135 FR-PET Resin  (discontinued **)
KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of p..
Arc Resistance 120 sec
120 sec
Average value: 120 sec Grade Count:6
Overview of materials for Polycarbonate, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp..
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical AP163 ABS, Permanent Anti-Static
Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance
Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical Lupox® GP1000A PBT
Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical Lupoy 1301EP22 Polycarbonate Resin
Description: LUPOY PC 1301EP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical Lupoy 1301V-7 Polycarbonate Resin
Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength..
Arc Resistance 120 sec
120 sec
ASTM D495
Gromax CCP PBT 1100-211X
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Arc Resistance 120 sec
120 sec
ASTM D495
Gromax CCP PBT 1100-630S
Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Arc Resistance 120 sec
120 sec
ASTM D495
Kolon Kopa® KN133 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
LG Chemical Lupoy 1302HP-09 Polycarbonate Resin
Description: LUPOY PC 1302HP-09 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten, PLC code 5; ASTM D 495
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten, PLC code 5; ASTM D 495
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Arc Resistance 120 sec
120 sec
ASTM D495
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
SABIC Innovative Plastics ULTEM MD131A PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
SABIC Innovative Plastics Valox® 4521 PBT
VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten, PLC code 5; ASTM D 495
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific)
Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
SABIC Innovative Plastics Xenoy® 5220U PBT+PC
Unreinforced PBT+PC Alloy. Impact Modified. Improved retention of mechanical properties under UV exposure. Excellent low temperature impact and chemical resistance.
Arc Resistance 120 sec
120 sec
ASTM D495
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer
PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3020IR is a high flow grade with added heat stabilizers, separating materials and stain..
Arc Resistance 120 sec
120 sec
ASTM D495
Samyang Trirex® 3027IR Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten, PLC code 5; ASTM D 495
SABIC Innovative Plastics Valox® 364 PBT
Designed for outdoor telecommunications enclosure applications.This data was supplied by SABIC-IP for the Americas region.
Arc Resistance 120 sec
120 sec
ASTM D495
Unitika UG-100-20 Engineering Plastic
Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd.
Arc Resistance 120 - 180 sec

@Thickness 3.00 mm
120 - 180 sec

@Thickness 0.118 in
UL Rating PLC 5 (120-180 sec)
Covestro Bayblend® T 64 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 65 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Ascend Performance Materials Vydyne® R543H Nylon 66, 43% Glass Filled, Dry as Molded
Vydyne® R543H is general-purpose, 43% glass-reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for improved machine feed, flow and mold release. ..
Arc Resistance 120 - 240 sec
120 - 240 sec
Average value: 172 sec Grade Count:24
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..
Arc Resistance 120 - 180 sec
120 - 180 sec
Tungsten; ASTM D495
SABIC Innovative Plastics ULTEM 1000 PEI (Asia Pacific)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer..
Copyright © lookpolymers.com All Rights Reserved