| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-FR2A-D Polycarbonate, Flame Retardant, Medium Flow Polycarbonate, Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-i.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-FR3A-D Polycarbonate, Flame Retardant, High Flow Polycarbonate, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
| Polymer Resources PC-UV1-D Polycarbonate, UV-stabilized, Low Flow Polycarbonate, UV-stabilized, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Po.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
| Polymer Resources TP-FR2 Polybutylene Terephthalate, Flame Retardant Polybutylene Terephthalate, Flame Retardant Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746 |
| Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
| PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
| PTS Tristar® PC-10R-(IM) 10 MFI Impact Modified Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 1.50 mm |
30 - 60 sec @Thickness 0.0591 in |
UL 746 |
| Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
| PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
PLC 2 |
| PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
| LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
| LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
| LG Chemical Lupoy 1301V-7 Polycarbonate Resin Description: LUPOY PC 1301V-07 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.60 mm |
30 - 60 sec @Thickness >=0.0630 in |
|
| LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
| LG Chemical LUPOY SR3108FM PC, Halogen Free Flame Retardance Description: Injection Molding, PC, Halogen Free Flame Retardance, Light Reflectance, White Color OnlyApplication: LCD Back Light Unit partsCAS: 103598-77-2, 9003-56-9 and 13463-67-1Information prov.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
| LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
| LG Chemical LUPOL GP3156F Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 84852-53-9, 14807-96-6 and 1309-64-4Information provided .. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
|
| LG Chemical Lupoy 1302HP-21 Polycarbonate Resin Description: LUPOY PC 1302HP-21 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=2.50 mm |
30 - 60 sec @Thickness >=0.0984 in |
|
| LG Chemical Lupoy 1302HP-22 Polycarbonate Resin Description: LUPOY PC 1302HP-22 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.60 mm |
30 - 60 sec @Thickness >=0.0630 in |
|
| LG Chemical Lupoy 1302UV-08 Polycarbonate Resin Description: LUPOY PC 1302UV-08 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.20 mm |
30 - 60 sec @Thickness >=0.0472 in |
|
| LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
| LG Chemical LUPOY GN5001RFJ PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (OA Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=3.00 mm |
30 - 60 sec @Thickness >=0.118 in |
All colors |
| Solvay Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness 3.00 mm |
30 - 60 sec @Thickness 0.118 in |
UL 746B |
| Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
| Hot Wire Ignition, HWI | 30 - 60 sec @Thickness >=1.50 mm |
30 - 60 sec @Thickness >=0.0591 in |
|
| LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||