Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : High Voltage Arc-Tracking Rate, HVTR = 0.394 in/min Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746A
SABIC Innovative Plastics Lexan® 915R PC (Asia Pacific)
Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties...
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746A
SABIC Innovative Plastics Lexan® 915RP PC (Asia Pacific)
Lexan* 915RP Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Polymer Resources NY6-GP1-[color]-H General Purpose Nylon 6, Heat Stabilized
General Purpose Nylon 6, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grade..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.05 mm
0.000 - 0.394 in/min

@Thickness 0.120 in
UL PLC 0 (0-10 mm/min)
Resinoid 1340 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.05 mm
0.000 - 0.394 in/min

@Thickness 0.120 in
UL PLC 0 (0-10 mm/min)
Resinoid 7051 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
PLC 0; UL 746
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. Ixef 1022..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL746A
Idemitsu Kosan Xarec® WA 210 SPS, 20% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified, Improved Mold Release. Used in Automotive and Industrial applications.
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL746A
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL746A
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746A
SABIC Innovative Plastics ULTEM 2312 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746A
SABIC Innovative Plastics Valox® 771 PBT
35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing.
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746A
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 1.47 mm
0.000 - 0.394 in/min

@Thickness 0.0579 in
UL PLC 0 (0-10 mm/min)
Sumitomo Bakelite North America RX® 2-520 Short-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 20NSP Nylon 66, DAM
Vydyne® 20NSP is a general-purpose, highly nucleated, lubricated PA66 resin available in natural color. It is designed to crystallize rapidly in order to reduce cycle times and increase productivit..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM
Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering ..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM
Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded
Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 64C-R Nylon 66, DAM
Vydyne® 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. Vydyne 64C-R resin offers high strength..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.05 mm
0.000 - 0.394 in/min

@Thickness 0.120 in
UL PLC 0 (0-10 mm/min)
Resinoid 1312 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.05 mm
0.000 - 0.394 in/min

@Thickness 0.120 in
UL PLC 0 (0-10 mm/min)
Resinoid 1322 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
BK
Hexion Bakelite™ EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Epoxy molding compound, inorganically filled, glass fiber reinforced, heat resistant, dimensionally stable, good electrical and mechanical properties, very good chemical resistance, low viscosity, U..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
BK
Hexion Bakelite™ PF 2874 Phenolic Formaldehyde Resin, Low Shrinkage, Improved Electrical Properties, UL Listed, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, increased mechanical strength, increased temperature stability, low water absorption, good dimensional stability, UL listed m..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min

@Thickness 3.00 mm
0.000 - 0.394 in/min

@Thickness 0.118 in
BK
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, DAM
Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding ..
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, DAM
Availability:Asia PacificEuropeNorth AmericaAdditive: Lubricant Features:Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood Tou..
Copyright © lookpolymers.com All Rights Reserved