| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | |
|
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer
Information provided by Polykemi AB
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Natural..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa HF-618 Flame Retardant ABS
Features:UL 94 V-0 @ 1.6-3.0mmHigh toughnessEasy flowApplications:Injection moldingShell of applianceCD-ROMPower switchInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa HR-527B Modified ABS
Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd...
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa JH830 Flame Retardant PC
Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy
Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa MAC-451 PC/ABS Alloy
Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingHousehold applianceAutomobile interior/exterior trim partsTel..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa MAC-601 PC/ABS Alloy
Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa MAC-751 HF PC/ABS Alloy
Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical ..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa PC-S609 Toughened PC
Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl..
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa PC-S809 Modified PC
Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Kingfa FRABS V-0 Flame Retardant ABS
Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd.
|
|||
| Back Pressure | 0.300 - 1.00 MPa | 43.5 - 145 psi | |
|
Kingfa MAC-551 PC/ABS Alloy
Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection molding |
|
Hexion UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Polyester molding compound, inorganically filled, glass fiber reinforced, styrene free, high dimensional stability, very slight post shrinkage, good mechanical properties, increased electrical value..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem AB860EM TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem AB870LG TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-860 TPE Compound
Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-945 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-950 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem GP-965B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem MP-8001 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem MP-930HD TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem SV-B87E TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection Molding |
|
Stellarchem 475-845N TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer
Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer
Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer
Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
|
|||
| Back Pressure | 0.500 - 1.00 MPa | 72.5 - 145 psi | Injection |
|
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer
Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,..
|
|||
| Back Pressure | 0.000 - 1.00 MPa | 0.000 - 145 psi | |
|
Solvay Specialty Polymers Ixef® 1313/0004 Polyarylamide, 40% Glass Fiber + Elastomer, DAM
(discontinued **)&l
Impact modified. The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manu..
|
|||