Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Glow Wire Test = 1520 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 825 °C

@Thickness 0.800 mm
1520 °F

@Thickness 0.0315 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer (Europe-Africa-Middle East)
Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Glow Wire Test 825 °C

@Thickness 1.00 mm
1520 °F

@Thickness 0.0394 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio..
Glow Wire Test 825 °C

@Thickness 2.00 mm
1520 °F

@Thickness 0.0787 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio..
Glow Wire Test 825 °C

@Thickness 2.50 mm
1520 °F

@Thickness 0.0984 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Glow Wire Test 825 °C

@Thickness 0.800 mm
1520 °F

@Thickness 0.0315 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer
Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1524 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1524 is a 50% glass-fiber reinforced, halogen-free flame retardant polyarylamide which exhibits high strength and stiffness, good surface gloss, and excellent creep resistance. - Black: Ixef 15..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® 18 R Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® 19 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® 19 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® 25 SR FD Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® 25 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® FC 23 UR Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 1.50 mm
1520 °F

@Thickness 0.0591 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® G2F 23 UR Polycarbonate-10% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 825 °C

@Thickness 0.800 mm
1520 °F

@Thickness 0.0315 in
ignition temperature; ISO 60695-2-13
Solvay TECHNYL® C 30H1 V30 Natural/F PA6, 30% glass fiber, DRY
Description: Flame retardant polyamide PA6, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This gr..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Glow Wire Test 825 °C

@Thickness 1.00 mm
1520 °F

@Thickness 0.0394 in
GWIT; IEC 60695-2-13
Covestro Makrolon® 2405 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low..
Glow Wire Test 825 °C

@Thickness 1.00 mm
1520 °F

@Thickness 0.0394 in
GWIT; IEC 60695-2-13
Covestro Makrolon® 2407 MAS056 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Improved impact streng..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow-Wire Ignition; IEC 60695-2-13
Eurostar Starflam RF0077P PA66/6, 35% Glass Filled, Injection Molded
Starflam RF0077P is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding Resin (also known as RF1007Z270EM)Information provided by Polym..
Glow Wire Test 824 °C

@Thickness 2.00 mm
1520 °F

@Thickness 0.0787 in
GWIT; IEC 60695
Eurotec® Tecomid® NA40 GR15 GR003 XA70 PA6.6, 15% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035
Information provided by Eurotec®
Glow Wire Test 825 °C

@Thickness 0.710 mm
1520 °F

@Thickness 0.0280 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 22HSP Nylon 66, General Purpose, Heat Stabilized, DAM
Availability:Asia PacificEuropeNorth America Additive:Lubricant Features: Fast Molding CycleGasoline ResistanceGeneral PurposeGood Abrasion ResistanceGood Chemical ResistanceGood Mold ReleaseGood To..
Glow Wire Test 825 °C

@Thickness 2.00 mm
1520 °F

@Thickness 0.0787 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East)
CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r..
Glow Wire Test 825 °C

@Thickness 1.00 mm
1520 °F

@Thickness 0.0394 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region.
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness a..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Ignition; IEC 60695-2-13
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)
Sorona® 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur..
Glow Wire Test 825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Copyright © lookpolymers.com All Rights Reserved