Polymer Property : Glow Wire Test = 725 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 725 °C

@Thickness 2.00 mm
1340 °F

@Thickness 0.0787 in
Ignition Temperature; IEC 60695-2-13
PolyOne OnFlex™ S HF 70A-3S1984 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Glow Wire Test 725 °C

@Thickness 2.00 mm
1340 °F

@Thickness 0.0787 in
Ignition Temperature; IEC 60695-2-13
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Glow Wire Test 725 °C

@Thickness 0.710 mm
1340 °F

@Thickness 0.0280 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 101L BKB080 Nylon 66  (Unverified Data**)
Zytel® 101L BKB080 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Glow Wire Test 725 °C

@Thickness 1.50 mm
1340 °F

@Thickness 0.0591 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf..
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 103FHS BKB009 Nylon 66  (Unverified Data**)
Zytel® 103FHS BKB009 is a heat stabilized, internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Perf..
Glow Wire Test 725 °C

@Thickness 0.710 mm
1340 °F

@Thickness 0.0280 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66  (Unverified Data**)
Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
DAM; Ignition; IEC 60695-2-13
DuPont Performance Polymers Zytel® 103HSL BKB080 Nylon 66  (Unverified Data**)
Zytel® 103HSL BKB080 is a heat stabilized, lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
Mitsubishi Xantar® C CM 506 U Polycarbonate/ABS Blend
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Glow Wire Test 725 °C

@Thickness 1.50 mm
1340 °F

@Thickness 0.0591 in
GWIT; IEC 60695-2-13
Lanxess Pocan® BF 4232 HR 901510 PBT, 30% Glass Fiber
PBT, 30% glass fiber, injection molding, flame retardant, hydrolysis stabilizedInformation provided by LANXESS.
Glow Wire Test 725 °C

@Thickness 1.00 mm
1340 °F

@Thickness 0.0394 in
GWIT
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Glow Wire Test 725 °C

@Thickness 2.00 mm
1340 °F

@Thickness 0.0787 in
GWIT
LATI Latamid 6 H2 G/20-V2HF PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Middle East; Asia Pacific; Euro..
Glow Wire Test 725 °C

@Thickness 1.60 mm
1340 °F

@Thickness 0.0630 in
ignition temperature; ISO 60695-2-13
Solvay TECHNYL® A 50H1 PA66, DRY
Description: Flame retardant polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applications: This phospho..
Glow Wire Test 725 °C

@Thickness 2.00 mm
1340 °F

@Thickness 0.0787 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Glow Wire Test 725 °C

@Thickness 1.60 mm
1340 °F

@Thickness 0.0630 in
ignition temperature; ISO 60695-2-13
Solvay TECHNYL® 52G1MX 25 Grey 7035 PA6, DRY
Description: Flame retardant polyamide PA6 reinforced with mineral filler for injection molding, also suitable for thin wall parts.Available in: Asia Pacific, Europe, Latin America and North America..
Glow Wire Test 725 °C

@Thickness 1.60 mm
1340 °F

@Thickness 0.0630 in
Glow Wire Ignition Temperature, dry; IEC 60695-2-13
DSM Akulon® CO-KGV4 /A JN.00.86 PA6-GF20 FR
% Glass Reinforced, Heat Stabilized, Flame Retardant (halogen-phosphorous-free)
Glow Wire Test 725 °C

@Thickness 0.800 mm
1340 °F

@Thickness 0.0315 in
Glow Wire Ignition Temperature, dry; IEC 60695-2-13
DSM Akulon® CO-KGV4 /A JN.00.86 PA6-GF20 FR
% Glass Reinforced, Heat Stabilized, Flame Retardant (halogen-phosphorous-free)
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature, dry; IEC 60695-2-13
DSM Akulon® K222-KMV5 /A PA6-MD25 FR(30)
25% Mineral Reinforced, Flame Retardant (Halogen free), Color Stabilized
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry)
Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie..
Glow Wire Test 725 °C

@Thickness 0.750 mm
1340 °F

@Thickness 0.0295 in
Glow Wire Ignition Temperature; IEC 60695-2-13
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Glow Wire Test 725 °C

@Thickness 0.750 mm
1340 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM
Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan..
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Glow Wire Test 725 °C

@Thickness 0.750 mm
1340 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Glow Wire Test 725 °C

@Thickness 1.50 mm
1340 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
Glow Wire Test 725 °C

@Thickness 1.50 mm
1340 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
Glow Wire Test 725 °C

@Thickness 0.750 mm
1340 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM
Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista..
Glow Wire Test 725 °C

@Thickness 0.810 mm
1340 °F

@Thickness 0.0319 in
DAM; Flammability Index; IEC 60695-2-12
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Glow Wire Test 725 °C

@Thickness 3.00 mm
1340 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..
Glow Wire Test 725 °C

@Thickness 0.710 mm
1340 °F

@Thickness 0.0280 in
Ignition Temperature; IEC 60695-2-12
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
Glow Wire Test 725 °C

@Thickness 1.50 mm
1340 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-12
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded
Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com..
Glow Wire Test 725 °C

@Thickness 1.00 mm
1340 °F

@Thickness 0.0394 in
GWIT
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri..