Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : SABIC Innovative Plastics (GE Plastics) > Category : Polybutylene Terephthalate (PBT) Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
SABIC Innovative Plastics Enduran 7062X PBT+PET (Asia Pacific) Polybutylene Terephthalate (PBT) Enduran
SABIC Innovative Plastics Lexan® LCR200 PBT+PC (Asia Pacific) Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Lexan®
SABIC Innovative Plastics LNP COLORCOMP W10009I PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP Colorcomp
SABIC Innovative Plastics LNP COLORCOMP WX96084 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP Colorcomp
SABIC Innovative Plastics LNP FARADEX WX94736 PBT Polybutylene Terephthalate (PBT) LNP FARADEX
SABIC Innovative Plastics REMEX VR4831 PBT Polybutylene Terephthalate (PBT)
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WAL34I PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT), Glass Bead Filled LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFI18 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL28 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP Lubricomp WFL32 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL36 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WG003 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WI001 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL002 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT Polybutylene Terephthalate (PBT), PTFE Filled LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics LNP LUBRICOMP WX95752L PBT (Asia Pacific) Polybutylene Terephthalate (PBT) LNP LUBRICOMP
SABIC Innovative Plastics Valox® 175 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 176 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 176HP PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 195 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 195HP PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 215HPR PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 295 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 305 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 308 PBT Polybutylene Terephthalate (PBT), Unreinforced, Molded Valox®
SABIC Innovative Plastics Valox® 309 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310HP PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310SE0 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 311 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 312 PBT Polybutylene Terephthalate (PBT), Unreinforced, Molded Valox®
SABIC Innovative Plastics Valox® 312 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 315 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 325 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 325M PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 337 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 357 PBT Polybutylene Terephthalate (PBT), Flame Retardant Valox®
SABIC Innovative Plastics Valox® 357 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 357 PBT+PC Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Valox®
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 357U PBT Polybutylene Terephthalate (PBT), Unreinforced, Molded Valox®
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 364 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 364 PBT+PC Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Valox®
SABIC Innovative Plastics Valox® 3706 PBT+PC Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced Valox®
SABIC Innovative Plastics Valox® 4012 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4012G PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 414 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420HP PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420M PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420SE0 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 420SE0U PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4521 PBT Polybutylene Terephthalate (PBT) Valox®
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) Polybutylene Terephthalate (PBT) Valox®
Copyright © lookpolymers.com All Rights Reserved