Category | Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) |
Manufacturer | SABIC Innovative Plastics (GE Plastics) |
Trade Name | LNP LUBRICOMP |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.40 g/cc | 0.0506 lb/in³ | ASTM D792 |
1.40 g/cc | 0.0506 lb/in³ | ISO 1183 | |
Moisture Absorption | 0.0700 % | 0.0700 % | 50% RH, 24 hrs; ASTM D570 |
Linear Mold Shrinkage, Flow | 0.026 - 0.028 cm/cm @Time 86400 sec |
0.026 - 0.028 in/in @Time 24.0 hour |
ASTM D955 |
Linear Mold Shrinkage, Transverse | 0.025 - 0.027 cm/cm @Time 86400 sec |
0.025 - 0.027 in/in @Time 24.0 hour |
ASTM D955 |
Melt Flow | 62 g/10 min @Load 5.00 kg, Temperature 250 °C |
62 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
45.0 MPa | 6530 psi | 5 mm/min; ISO 527 | |
Tensile Strength, Yield | 43.0 MPa | 6240 psi | Type I, 5 mm/min; ASTM D638 |
45.0 MPa | 6530 psi | 5 mm/min; ISO 527 | |
Elongation at Break | 14 % | 14 % | Type I, 5 mm/min; ASTM D638 |
18.9 % | 18.9 % | 5 mm/min; ISO 527 | |
Elongation at Yield | 11 % | 11 % | Type I, 5 mm/min; ASTM D638 |
17.8 % | 17.8 % | 5 mm/min; ISO 527 | |
Tensile Modulus | 2.55 GPa | 370 ksi | 50 mm/min; ASTM D638 |
2.68 GPa | 389 ksi | 1 mm/min; ISO 527 | |
Flexural Yield Strength | 74.0 MPa | 10700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
74.0 MPa | 10700 psi | 2 mm/min; ISO 178 | |
Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
2.40 GPa | 348 ksi | 2 mm/min; ISO 178 | |
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
Izod Impact, Notched (ISO) | 4.00 kJ/m² | 1.90 ft-lb/in² | 80*10*4; ISO 180/1A |
Izod Impact, Unnotched (ISO) | 44.0 kJ/m² | 20.9 ft-lb/in² | 80*10*4; ISO 180/1U |
Coefficient of Friction, Dynamic | 0.33 | 0.33 | ASTM D3702 Modified |
Coefficient of Friction, Static | 0.24 | 0.24 | ASTM D3702 Modified |
K (wear) Factor | 10.1 x 10-8 mm³/N-M | 5.00 x 10-10 in³-min/ft-lb-hr | Washer; ASTM D3702 Modified |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 55.0 °C @Thickness 3.20 mm |
131 °F @Thickness 0.126 in |
unannealed; ASTM D648 |