Material Notes:
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact compliant, color black.Typical Application Areas: Complex geometries with thin cross sections or long flow length where higher strength in a static or dynamic system is required. Excellent wear resistance, low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.Information provided by Victrex.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption at Saturation 0.30 %

@Temperature 23.0 °C
0.30 %

@Temperature 73.4 °F
immersion; ISO 62-1
0.45 %

@Temperature 100 °C
0.45 %

@Temperature 212 °F
immersion; ISO 62-1
Viscosity 300000 cP

@Temperature 400 °C
300000 cP

@Temperature 752 °F
melt; ISO 11443
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4
Spiral Flow 14.0 cm

@Thickness 1.00 mm
5.51 in

@Thickness 0.0394 in
recommended processing conditions
Mechanical Properties Metric English Comments
Hardness, Shore D 87.5
87.5
ISO 868
Tensile Strength at Break 60.0 MPa

@Temperature 275 °C
8700 psi

@Temperature 527 °F
ISO 527
105 MPa

@Temperature 175 °C
15200 psi

@Temperature 347 °F
ISO 527
170 MPa

@Temperature 125 °C
24700 psi

@Temperature 257 °F
ISO 527
270 MPa

@Temperature 23.0 °C
39200 psi

@Temperature 73.4 °F
ISO 527
Elongation at Break 1.5 %
1.5 %
ISO 527
Tensile Modulus 28.0 GPa
4060 ksi
ISO 527
Flexural Strength 65.0 MPa

@Temperature 275 °C
9430 psi

@Temperature 527 °F
ISO 178
130 MPa

@Temperature 175 °C
18900 psi

@Temperature 347 °F
ISO 178
275 MPa

@Temperature 125 °C
39900 psi

@Temperature 257 °F
ISO 178
380 MPa

@Temperature 23.0 °C
55100 psi

@Temperature 73.4 °F
ISO 178
Flexural Modulus 24.0 GPa
3480 ksi
ISO 178
Compressive Strength 70.0 MPa

@Temperature 200 °C
10200 psi

@Temperature 392 °F
ISO 604
200 MPa

@Temperature 120 °C
29000 psi

@Temperature 248 °F
ISO 604
300 MPa

@Temperature 23.0 °C
43500 psi

@Temperature 73.4 °F
ISO 604
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
ISO 180/U
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
ISO 179/1U
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C
22.2 µin/in-°F
Average below Tg; ISO 11359
100 µm/m-°C
55.6 µin/in-°F
Average above Tg; ISO 11359
CTE, linear, Parallel to Flow 5.00 µm/m-°C
2.78 µin/in-°F
Below Tg; ISO 11359
6.00 µm/m-°C
3.33 µin/in-°F
Above Tg; ISO 11359
Thermal Conductivity 0.950 W/m-K
6.59 BTU-in/hr-ft²-°F
Average; ISO 22007-4
2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Along flow; ISO 22007-4
Melting Point 344 °C
651 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 339 °C
642 °F
ISO 75-f
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
147 °C
297 °F
Midpoint; ISO 11357
UL RTI, Mechanical with Impact 200 °C
392 °F
UL 746B
UL RTI, Mechanical without Impact 240 °C
464 °F
UL 746B
Glow Wire Test 960 °C

@Thickness 2.00 mm
1760 °F

@Thickness 0.0787 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1e+05
1e+05
1V; ASTM D4496
Processing Properties Metric English Comments
Processing Temperature <= 100 °C
<= 212 °F
Hopper Temperature
Nozzle Temperature 385 °C
725 °F
Mold Temperature 180 - 210 °C
356 - 410 °F
Dry Time 3.00 hour

@Temperature 150 °C
3.00 hour

@Temperature 302 °F
5.00 hour

@Temperature 120 °C
5.00 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Toxicity Index 0.05
CO content
0.12
CO2 content
0.17
Total gases
Copyright © lookpolymers.com All Rights Reserved