Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 270 MPa @Temperature 23.0 °C |
39200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Tensile Strength at Break | 270 MPa @Temperature 23.0 °C |
39200 psi @Temperature 73.4 °F |
ISO 527 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |