Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 147 °C | 297 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical propert.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150UF10 Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, .. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | |
Cookson Group Plaskon® AMC2 (132.203) Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound specifically formulated for packaging stress-sensitive devices in DIPs, SOICs, PLCCs and small QFPs. F.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-880 CF30 Polyetheretherketone (PEEK), 30% Carbon Fiber KetaSpire® KT-880 CF30 is a high flow, 30% carbon fiber reinforced grade of polyetheretherketone (PEEK). Carbon-fiber reinforcement of KetaSpire® PEEK provides the maximum levels of mechanical.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK) KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK) KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK), 30% Glass Fiber KetaSpire® KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaS.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Ultimate Tg |
Tra-Con Tra-Bond 161-3 Temperature Resistant Epoxy Adhesive TRA-BOND 161-3 two component, premixed and frozen, epoxy adhesive is highly filled. This electrically insulating adhesive provides structural strength to 150°C and semi structural strength to 300°.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2408 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | ISO 11357-1/-2 |
Covestro Makrolon® LTG2623 Polycarbonate PreprocessingMax. Water content |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | ISO 11357-1/-2 |
Covestro Makrolon® DP1-1843* Polycarbonate ISO 7391-PC,RL,(,,)-09-9Developmental productMVR (300 °C/1.2 kg) 9.5 cm3/10 minMedium viscosityUV stabilizedRotomoldingAvailable in transparent and translucent colorsGlobe lightsAs of 1 September 2.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |
|||
Glass Transition Temp, Tg | 147 °C | 297 °F | Midpoint; ISO 11357 |
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co.. |