Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Flexural Strength | 380 MPa @Temperature 23.0 °C |
55100 psi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Flexural Strength | 380 MPa @Temperature -40.0 °C |
55100 psi @Temperature -40.0 °F |
Practical Use (Water Absorption 0.8%); ASTM-D790 |
Toyobo GLAMIDE® TY-592GHV 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 380 MPa @Treatment Temp. 100 °C, Time 3600 sec |
55100 psi @Treatment Temp. 212 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Flexural Strength | 380 MPa @Treatment Temp. 250 °C, Time 3600 sec |
55100 psi @Treatment Temp. 482 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |