Polymer Property : Flexural Strength = 65.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 65.0 MPa

@Temperature 275 °C
9430 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c..
Flexural Strength 65.0 MPa

@Temperature 275 °C
9430 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Flexural Strength 65.0 MPa

@Temperature 225 °C
9430 psi

@Temperature 437 °F
ISO 178
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont..
Flexural Strength 65.0 MPa

@Strain 8.00 %
9430 psi

@Strain 8.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced
PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS.
Flexural Strength 65.0 MPa

@Strain 8.00 %
9430 psi

@Strain 8.00 %
Conditioned; ISO 178
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral
PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties
Flexural Strength 65.0 MPa

@Temperature -40.0 °C
9430 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 65.0 MPa

@Thickness >=1.50 mm
9430 psi

@Thickness >=0.0591 in
1hr/130°C/measured at 130°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Flexural Strength 65.0 MPa

@Thickness >=1.50 mm
9430 psi

@Thickness >=0.0591 in
1hr/130°C/measured at 130°C; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..