Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 143 - 150 °C | 289 - 302 °F | Average value: 145 °C Grade Count:5 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150PF Easy Flow Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Glass Transition Temp, Tg | >= 143 °C | >= 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Glass Transition Temp, Tg | >= 143 °C | >= 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650P PolyEtherEtherKetone High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating VICOTE 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for low.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DIN 53 765 |
Ensinger Tecapeek® ID Metal Detectable Polyetheretherketone Tecapeek™ ID metal detectable polyetheretherketone, made from Victrex® PEEK 450G polymer, is formulated to reduce the risk of product contamination and allow for easy detection of fragments in the.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Ensinger Tecapeek® XP-96 Compression Molded PEEK Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | dynamic; DIN 53 736 |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 706 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 705 Blue Polyetheretherketone (PEEK) Powder Coating VICOTE 705 Blue is a blue pigmented version of the VICOTE 705 grade and contains additives to help with adhesion, wetting of the substrate and shrinkage. This grade has a nominal particle size of ~ .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 705 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 707 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |