Chase Plastics CP Pryme® NN300TL (Dry) Nylon 66, Lubricated, Impact Modified, Recycled Content

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® NN300TL (Dry) Nylon 66, Lubricated, Impact Modified, Recycled Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Impact modifiedGood toughnessLubricatedRecycled ContentForm: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
At 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
0.125 in; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 64.1 MPa
9300 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 2.07 GPa
300 ksi
ASTM D790
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
0.125 in; ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 °C
491 °F
Deflection Temperature at 0.46 MPa (66 psi) 221 °C
430 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.3 °C
164 °F
Unannealed; ASTM D648